Sign In | Join Free | My polstate.com
China Baoji City Changsheng Titanium Co.,Ltd logo
Baoji City Changsheng Titanium Co.,Ltd
Baoji City Changsheng Titanium Co., Ltd
Verified Supplier

4 Years

Home > Tantalum Products >

Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant

Baoji City Changsheng Titanium Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant

Brand Name : Changsheng

Model Number : R05200

Certification : ISO 9001;2015

Place of Origin : China

MOQ : 1kg

Price : USD420/kg

Payment Terms : L/C, T/T, Western Union, MoneyGram,paypal

Supply Ability : 500kgs/month

Delivery Time : 15-30days

Packaging Details : Stardard export package

Original Place : CHINA

Packing : Standard wooden case

Electrical Conductivity : 0.13 x 10^6 S/m

Process : Mixing

Port : Tianjin,Qingdao and Shanghai

Product Standard : ASTM B 365-98

Conditions : Annealed

Atomic Mass : 180.94788 g/mol

Commodity : Tantalum tube

Corrosion Resistance : outstanding

Boiling Point : 5425°C

Specifications : customized

Application : electronics, chemicals

Evaporation Heat : 743kJ/mol

Shape : Crucible,as per drawing

Contact Now

Description

Tantalum rod is a rod shaped product made of tantalum tungsten alloy, The numbers are Ta1, Ta2. Implementation standard: ASTM B 365 GB/T26012-2010 or according to Beijing Oriental Color tantalum Niobium enterprise standard execution,the density of tantalum rod is usually greater than or equal to 16.6g/cm³, the supply state is polished surface, the size range can start from Φ0.15xL, can be customized according to customer requirements. Tantalum rods have high melting point (about 3000 degrees Celsius), good corrosion resistance, high density (about 16.6 g/cm ³) and other characteristics.

Product photo

Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant

Application

For the production of vacuum blast furnace heating parts, heat insulation parts and charging vessels, in the chemical industry can be used to make digesters, heaters,

Coolers, all kinds of utensils and devices, as well as in aviation, aerospace industry, medical equipment and other fields are widely used.

Chemical Composition

Grade chemical composition %, max
Fe Si Ni W Mo Ti Nb O C H N Ta
Ta 1 0.005 0.005 0.005 0.005 0.002 0.002 0.005 0.02 0.004 0.002 0.005 remain
Ta 2 0.005 0.005 0.005 0.005 0.002 0.002 0.1 0.03 0.1 0.002 0.01 remain

FRQ

Commercial CE SAA ROHS Certificate Outdoor IP65 Waterproof 20W 30W 50W 100W 200W 12V LED Flood Lights

Q1. Can I have a sample order for led light?

A: Yes, we welcome sample order to test and check quality. Mixed samples are acceptable.

Q2. What about the lead time?

A: 3-5 days for Sample preparing ,8-10 working days for mass production.

Q3. Do you have any MOQ limit for led light order?

A: Low MOQ, 1pc for sample checking is available.

Q4. How do you ship the goods and how long does it take to arrive?

A: Ship by DHL, UPS, FedEx or TNT. It takes 3-5 days to arrive. Airline and sea shipping also optional.

Q5. How to proceed an order for led light?

A: Firstly let us know your requirements or application.

Secondly We quote according to your requirements or our suggestions.

Thirdly customer confirms the samples and places deposit for formal order.

Fourthly We arrange the production.

Q6. Is it OK to print my logo on led light product?

A: Yes. Please inform us formally before our production.

Q7: Do you offer guarantee for the products?

A: Yes, we offer 5 years warranty to our products.

Q8: How to deal with the faulty?

A: Firstly, Our products are produced in strict quality control system and the defective rate will be less than 0.2%.

Secondly, during the guarantee period, we will send new lights with new order for small quantity. For defective batch products, we will repair them and resend them to you or we can discuss the solution including re-call according to real situation.


Product Tags:

Superalloy Tantalum Rods Bars

      

Artificial Bone Implant Tantalum Rods Bars

      

R05200 Tantalum Rods Bars

      
Wholesale Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant from china suppliers

Tantalum Rods Bars R05200 Ta1 Ta2 Superalloy Artificial Bone Implant Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Baoji City Changsheng Titanium Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)